Environmental Friendly LSZH Low smoke zero halogen sheathing material do not contain halogens and do not produce toxic gases when burned. Thus reducing harm to the environment and human body. The amount of smoke produced by low smoke halogen-free sheathing materials during combustion is much lower than that of traditional cable sheathing materials such as PVC, which helps to improve visibility during fires and facilitates personnel evacuation and fire rescue. The low smoke halogen-free sheathing material complies with RoHS environmental protection standards.
- Good flame retardancy;
- Low toxicity and low corrosion;
- Environmental Friendly lszh low smoke zero halogen material has heat and cold resistance;
- Excellent processing performance;
- Good mechanical properties. Such as tensile strength and elongation at break, can meet the use requirements of cables in different application scenarios;
- Good oil resistance;
- LSZH Low smoke zero halogen Cable sheath material is suitable for cable lines in transportation projects such as subways, high-speed railways, highways, bridges, etc.;
- Widely used in communication systems such as telephones, computers, and networks;
- Low smoke halogen-free sheathing materials are also often used in cable lines in power systems. Such as power generation, transmission, substation, and distribution;
T-PO(12) Series Irradiation Crosslinking Low Smoke Halogen-Free Flame Retardant Polyolefin Oil Resistance Cable Material Products For Marine
Suitable For Marine Cables, With Excellent Oil Resistance And Compliance With Iec-60092 Standards.
| Typical Physical And Mechanical Properties Are As Follows: |
| Item |
|
Unit |
Test Method |
Typical |
| Density |
|
g/cm3 |
GB/T 1033-2008 |
1.46 |
| Tensile Strength |
|
Mpa |
GB/T 1040-2006 |
13.2 |
| Elongation At Break |
|
% |
GB/T 1040-2006 |
185 |
| Air Thermal Aging Performance |
|
ºC×day |
GB/T 2951.7 |
100×7 |
| Maximum Change Rate Of Tensile Strength |
|
% |
GB/T 2951.7 |
-11 |
| Maximum Change Rate Of Elongation At Break |
|
% |
GB/T 2951.7 |
-6 |
| Smoke Density |
Without Flames |
… |
GB/T8323-2008 |
175 |
| With Flames |
… |
59 |
| Oxygen Index |
|
% |
GB/T 2406-2009 |
34 |
| Low Temperature Impact Embrittlement Temperature (-20 ºC) |
|
Failure Count |
GB/T 5470-2008 |
Pass |
| Thermal Deformation (90 ºC, 4h) |
|
% |
GB/T 8815 |
8 |
| Dielectric Strength |
|
MV/m |
GB/T 1408.1 |
29 |
| 20 ºC Volume Resistivity |
|
Ω·m |
GB/T 1410-2006 |
1.9×1010 |
| PH Value |
|
|
IEC60754-2 |
5.9 |
| Conductivity |
|
μs/cm |
IEC60754-2 |
2 |
| Halogen Gas Content |
|
mg/g |
IEC60754-2 |
1.2 |
| Toxicity Index |
|
… |
NES 713 |
1.4 |
*Appearance: Uniform color and no impurities. Evaluation: Qualified, meeting the requirements specified by ROHS.
Note: The above typical values are random sampling data. |
Packaging Storage And Transport
The material must be supplied packaged in such a way as to be protected during transport, handling and storage. The packaging must be in plastic bags, "bigbag", or cardboard box. The packaging must have adequate strength and be free of impurities that may contaminate the product and be protected against moisture as well.


What We Have In The Field Of Telecom Optical & Electric Cable :
1>Mature and Efficient Supply Chain System And Rich Industrial Resources
2>Complete Materials Demand Solutions For Cable Manufacturing And Technical Services
3>Overall Solutions And Customized Services In Factory Design, Equipment Configuration, Product Development And Rawmaterial Supply
*Quotation Varies According To Customer's Requirements And Quantity Of Products